Details
- Annealing bag suitable for powder nitriding, boriding and high speed steel hardening up to approx. 1050 °C - 1150 °C for cold work purposes
- Made of stainless steel heat treating foil for single use
- For hardening of blocks, stamps, cutting plates, etc.
- Rapid heating binds the oxygen in the annealing bag so that high-alloy and medium-alloy steel grades can be hardened
- Rapid quenching in air, oil or water, ensuring high dimensional accuracy
- Workpieces are placed as tightly as possible into the annealing bag
- Airtight lock by means of folds of a fold lock or suitable tools
Quadratic cross-section | Rectangular cross-section | |||||||
---|---|---|---|---|---|---|---|---|
Article no. | Dimensions in mm | Article no. | Dimensions in mm | |||||
W | D | H | W | D | H | |||
491063520 | 40 | 200 | 40 | 491041520 | 100 | 200 | 25 | |
491063530 | 40 | 300 | 40 | 491041530 | 100 | 300 | 25 | |
491064520 | 60 | 200 | 60 | 491043030 | 150 | 300 | 25 | |
491064530 | 60 | 300 | 60 | 491043520 | 150 | 200 | 40 | |
491065520 | 80 | 200 | 80 | 491043550 | 150 | 500 | 40 | |
491065530 | 80 | 300 | 80 | 491045030 | 200 | 300 | 40 | |
491066520 | 100 | 200 | 100 | 491045242 | 200 | 420 | 100 | |
491066545 | 100 | 450 | 100 | 491046535 | 250 | 350 | 40 |